High Permeability Mn-Zn Ferrite Core Magnet

High Permeability Mn-Zn Ferrite Core Magnet

Description Mn-Zn Soft Ferrite Cores Mn-Zn ferrite core is consist of a combination of iron oxide and strontium carbonate. Thanks to their low cost, light weight, relatively high energy products and good anti-demagnetization , ferrite and ceramic magnets are widely used. The ferrite and ceramic...

Send Inquiry

Product Details

Description

Mn-Zn Soft Ferrite Cores 
Mn-Zn ferrite core is consist of a combination of iron oxide and strontium carbonate. Thanks to their low cost, light weight, relatively high energy products and good anti-demagnetization , ferrite and ceramic magnets are widely used. The ferrite and ceramic magnets (Mn-Zn ferrite cores) have a maximum operating temperature of 480 ° F, which is ideal for some high temperature applications. Common applications include: loudspeaker magnets, motors, metallic reed switches and hall effect devices.

Material Characteristics of MnZn Power Ferrite

Grade

Initial Permeability

μi

Saturation Flux Density

BS(mT)

1194 A/m

Core Loss

Pcv(kW/m3

100kHz、200mT

Curie Temperature
(℃)

Density
( kg/m3

25℃

100℃

140℃

25℃

60℃

100℃

120℃

140℃

CYP–4

2400±25%

500

390

-

600

460

410

-

-

>215

4.8x103

CYP–4T

(new)

1800±25%

520

430

360

900

-

500

-

400

>240

4.8x103

CYP–44

2400±25%

510

390

-

600

400

300

380

-

>215

4.8x103

CYP–44A

2400±25%

530

410

-

600

400

280

380

-

>215

4.8x103

CYP–44C

2400±25%

530

420

-

550

380

250

360

-

>215

4.8x103

CYP–44B

2400±25%

510

390

-

300

550

-

150

350

-

-

>215

4.8x103

CYP–5A

1400±25%

490

390

-

130

160

80

130

80

130

110

160

-

>250

4.7x103

CYB–60
(new)

1000±25%

580

490

-

1200

-

650

-

-

>300

4.9x103

CYP–90

2200±25%

540

450

-

680

-

320

-

-

>250

4.9x103

CYP–95

3300±25%

530

410

-

350

290

300

360

-

>215

4.8x103

CYP–95A

3300±25%

530

410

-

330

280

290

350

-

>215

4.8x103

CYP–95B

3300±25%

530

410

-

310

280

290

340

-

>215

4.8x103

CYP–96

3000±25%

540

450

-

360

310

300

350

-

>250

4.9x103

CYP–97

3000±25%

530

410

-

380

320

300

320

380

>215

4.8x103

Test core:OD=25mm  TH=8mm  ID=15mm

Ⅰ Test Conditions:200kHz、100mT; ⅡTest Conditions:300kHz、100mT; 

Ⅲ Test Conditions:500kHz、50mT; ⅣTest Conditions:1MHz、30mT。 

MnZn High Permeability/High Impedance Ferrite Material Characteristics

Grade

Initial Permeability
μi

 

Saturation Flux Density
Bs(mT)

Relative Loss Factor
tanδ/μi

Electric   Resistivity
ρ

Ω·m

Curie Temperature

(℃)

Density

( kg/m3

25℃、1194 A/m

x10-6(10kHz)

CYH–5

5000±25%

450

3.5

0.5

>135

4.8x103

CYH–5T
(new)

5500±25%

460

2.5

0.5

>160

4.85x103

CYH–7F

7000±25%

430

6.5

0.15

>125

4.9x103

CYH–10F

10000±30%

420

1.6

0.3

>120

5.0x103

CYH–12F

12000±30%

400

1.6

0.3

>110

5.0x103

CYH–15F
(new)

15000±30%

400

1.6

0.3

>105

5.0x103

CYB–45

4200±25%

470

3

2

>160

4.85x103

PRODUCTION PROCESS FLOWCHART

PRODUCT ADVANTAGE

QUALITY


APPLICATIONS

Mn-Zn Soft Ferrite Cores 
Productions are mainly used in: switching power supply, telecommunication, household appliances, anti-electromagnetic interference (EMI) etc.

Inquiry